Cast Iron Metal Fatigue Failure

July 28, 2011 By Tom Read Leave a Comment

California failure analysis expert performs a failure analysis on a failed cast iron “latch lever” from a wood stove. This failure initiated as a fatigue crack at a casting defect. It progressed as a fatigue crack through most of the thickness until the final overload failure. Upper left is a photograph of the backside of […]

Filed Under: Failure Analysis Tagged With: Cast Iron, Casting Defect, Latch Lever, Metal Fatigue, Wood Stove

Read Consulting Failure Analysis

Thomas L. Read, PhD,
1435 Fulton Road Santa Rosa, CA
Phone: 707-494-5089
email: info@readconsulting.com

Subscribe to Articles & White Papers

Enter your email address to subscribe to this blog and receive notifications of new posts by email.

  • Home
  • About
  • Experience
  • Expertise
  • Laboratory
  • Failure Analysis
  • Blog
  • White Papers

Read Consulting Failure Analysis

Thomas L. Read, PhD,
1435 Fulton Road Santa Rosa, CA
Phone: 707-494-5089
email: info@readconsulting.com

Connect With Read Consulting

FacebookTwitterLinkedinYouTubeRSS Feed

Registered Professional Engineer

Thomas L. Read, PhD., CEO
Registered Professional Engineer
Certificate No. MF002174
State of California.

Copyright © 2022 Read Consulting · Materials Failure Analysis And Process Engineering