Brass Plumbing Failure Analysis Stress Corrosion Cracking (SCC)

October 21, 2011 By Tom Read Leave a Comment

California failure analysis expert witness has analyzed numerous plumbing failures involving yellow brass (i.e. brass with more than 30% Zn in the alloy). The two major brass failure modes in yellow brass are dezincification and stress corrosion cracking. Above are two samples of stress corrosion cracking. Sress corrosion of yellow brass commonly involves the presence of ammonia along with the […]

Filed Under: Failure Analysis Tagged With: Brass, Cracking, Plumbing, Stress Corrosion

Read Consulting Failure Analysis

Thomas L. Read, PhD,
1435 Fulton Road Santa Rosa, CA
Phone: 707-494-5089
email: info@readconsulting.com

Subscribe to Articles & White Papers

Enter your email address to subscribe to this blog and receive notifications of new posts by email.

  • Home
  • About
  • Experience
  • Expertise
  • Laboratory
  • Failure Analysis
  • Blog
  • White Papers

Read Consulting Failure Analysis

Thomas L. Read, PhD,
1435 Fulton Road Santa Rosa, CA
Phone: 707-494-5089
email: info@readconsulting.com

Connect With Read Consulting

FacebookTwitterLinkedinYouTubeRSS Feed

Registered Professional Engineer

Thomas L. Read, PhD., CEO
Registered Professional Engineer
Certificate No. MF002174
State of California.

Copyright © 2022 Read Consulting · Materials Failure Analysis And Process Engineering