Rubber Failure Analysis: Rubber Seal Failure Analysis

January 22, 2012 By Tom Read Leave a Comment

A California failure expert witness was asked to determine the root cause of a rubber gasket leak. The molded rubber gasket seal was integrated into a hydraulic lift operating at 650 psi. Over time it had developed a very small hole and approximately 60 gallons of hydraulic oil escaped through this small leak. Read Consulting Failure […]

Filed Under: Failure Analysis Tagged With: Leak, Molding Defect, Rubber Gasket, Rubber Seal

Plastic Failure Analysis

October 27, 2008 By Tom Read Leave a Comment

Plastics failure expert performs a root cause failure analysis on a plastic automobile door handle. The handle is from a van’s sliding side door. The product failure occurred when the user was trying to close the van’s sliding door. This is a products liability issue because the handle failed in a brittle manner and a […]

Filed Under: Failure Analysis Tagged With: Automobile, Door Handle, Manufacturing Defects, Molding Defect, Plastic Failure

Read Consulting Failure Analysis

Thomas L. Read, PhD,
1435 Fulton Road Santa Rosa, CA
Phone: 707-494-5089
email: info@readconsulting.com

Subscribe to Articles & White Papers

Enter your email address to subscribe to this blog and receive notifications of new posts by email.

  • Home
  • About
  • Experience
  • Expertise
  • Laboratory
  • Failure Analysis
  • Blog
  • White Papers

Read Consulting Failure Analysis

Thomas L. Read, PhD,
1435 Fulton Road Santa Rosa, CA
Phone: 707-494-5089
email: info@readconsulting.com

Connect With Read Consulting

FacebookTwitterLinkedinYouTubeRSS Feed

Registered Professional Engineer

Thomas L. Read, PhD., CEO
Registered Professional Engineer
Certificate No. MF002174
State of California.

Copyright © 2022 Read Consulting · Materials Failure Analysis And Process Engineering