Read Consulting failure analysis laboratory performed a glass failure analysis of a broken of vinaigrette salad dressing bottle. The bottle top broke off when the top was being twisted off and injured the user. The integrity of the bottle neck was in question. There was a suspicion of a glass defect in the bottle neck […]
Diamond Tool Design{ Glass Expert Discusses Glass Damage From Diamond Grinding
Chart Showing Damage Depth of Diamond Grind v. Diamond Particle Size Checks in Glass Revealed by Etching with Buffered HF 100 Grit Damage Remaining After 0.0075″ Had Been Removed Certain types of glass must be ground to shape with a diamond tool, and they are then lapped and polished to make them transparent. If this […]